Anti-yellowing additives are specially developed modified composite additives for high-temperature resistant powder coatings; this product is a specialized additive developed for high-temperature resistance purposes, capable of achieving high-temperature powder coating effects at 300-700 degrees, and demonstrates excellent high-temperature resistance in powder coating systems.

The coating formed after heating and cross-linking of the product has a fine surface, smooth and even; pencil hardness is 1H when the surface is undamaged; after prolonged high-temperature baking, it still maintains excellent adhesion and outstanding gloss retention; it does not decompose when stored long-term in powder coatings and does not affect the storage stability of the powder coatings.

Product code   Application PerformanceRecommended dosage
PTN501Resistant to yellowing in gas furnaces, and has good anti-yellowing performance under 230℃ baking conditions0.3-1%
pre-blending
PTN502Resistant to yellowing in gas furnaces and high temperatures, the light white powder has little color difference when  baked at 2500.3-1%
pre-blending
PTN503Significantly inhibits the yellowing of light white powder caused by gas furnace and high temperature baking0.3-1%
pre-blending
PTN504Resistant to yellowing in gas furnaces and high temperatures, the light white powder has little color difference when baked at 3000.3-1%
pre-blending
PTN505Special anti-yellowing agent for HAA system, effectively improving the yellowing phenomenon caused by the coating's resistance to gas and high-temperature baking0.5-1.5% 
pre-blending
PTN506Used for 300/600 degree high temperature powder coating to improve the stability of the coating under high temperature baking2-5%
pre-blending
PTN507Used for 500/700 degree high temperature powder coating to improve the stability of the coating under high tempera-ture baking2-5%
pre-blending
PTN508Used for 500/700 degree high temperature powder coating to improve the stability of the coating under high tempera-ture baking2-5%
pre-blending